For detailed information, other images and documents, please select individual articles from the following table.
AKASEL Demo kit for superalloys with diffusion layers
Sample preparation in metallography
Products
Application
Demo kit for sample preparation of superalloys with diffusion layers. Contains all the consumables that will be required to carry out a specific preparation for these materials. Includes the preparation guide Aka-Brief.
Execution
- Consisting of:
- 2-in-1 diamond suspension DiaUltra 3 µm
- 2-in-1 diamond suspension DiaUltra 9 µm
- Fumed silica suspension 0.2 µm, alkaline
- Diamond grinding disc Aka-Piatto 120
- Diamond lapping disc Aka-Allegran 9
- Dressing stone #220, 25 mm x 25 mm x 150 mm
- Self-adhesive polishing cloth Aka-Chemal
- Self-adhesive polishing cloth Aka-Silk
Notes
Individual components from this demo kit can be found in our online shop under "Accessories"
Select RAL-colour code